Crazing: Why the Same Crack Pattern Means Different Things in Different Materials

Crazing describes networks of fine surface features, but its physical meaning depends on the material. In ceramic glaze it usually means a network of cracks in the glaze layer. In polymers, a craze can be a local zone of voids bridged by stretched fibrils before it becomes an open crack. Concrete surface crazing involves another mechanism again.

Start with the affected material
ObjectMeaning to investigateGo to
Glazed ceramicCracks in the glaze layer and its relationship to the body.Ceramic glaze
PlasticVoids bridged by fibrils, often associated with stress and environmental exposure.Polymer crazing
ConcreteA network of fine, shallow surface cracks.Concrete surface

First identify the material and the layer

A web of fine lines on a glazed mug, a stressed clear plastic cover and a concrete floor may look similar at arm’s length. They should not receive the same diagnosis or treatment. The Museum of Fine Arts Boston’s CAMEO entry records how the term spans several materials.

On a glazed ceramic

The glaze is a glassy layer bonded to a ceramic body. Differences in their dimensional response during cooling or subsequent use can put the glaze into tension and produce fine cracks. The US National Park Service museum handbook explains glaze crazing in the context of ceramic care.

A crack in the glaze does not necessarily extend through the entire body. However, the network can allow staining or access to a porous body. Appearance alone cannot establish whether a particular vessel is suitable for food use.

In a transparent polymer

IUPAC defines polymer crazing in terms of cavities spanned by load-bearing fibrils. A craze is therefore a damage zone where highly stretched material spans microscopic voids. Light scattering can make the zone look white or silvery. It can carry some load temporarily, but it is not undamaged plastic; the fibrils can fail and the craze can develop into a crack.

Stress, polymer structure, temperature and chemical environment influence the process. A cleaning solvent can change a stressed plastic’s behaviour, so transferring a cleaning method from glass to an unknown clear polymer is a poor assumption.

On concrete

Fine shallow crack networks can develop in a surface layer through shrinkage-related effects. NRMCA’s Concrete in Practice collection includes a dedicated guide, CIP 3, for concrete surface crazing. That is a different context from a glaze pulling against a ceramic body.

What a photograph cannot settle

Scale, depth, recent growth and loading matter. A photo may show the pattern while hiding whether the cracks are superficial, growing or connected to a larger failure. Structural safety and food-contact suitability require information beyond an attractive close-up.

Record when the pattern appeared, whether it changes, what the object is made from and any recent heat, load or chemical exposure. On a historical object, avoid rubbing pigment or liquid into cracks simply to make them visible.

The crack-tip discussion in brittle ceramic fracture explains why a small defect can matter mechanically. For a different type of evolving surface damage, bronze disease shows why ongoing material loss must be distinguished from an old, stable appearance.

Scroll to Top